More info
Recovery:
Could obtain above 95% recovery of the alloying element in around 15 minutes after addition of the material to a stirred bath between 720 ºC and 750 ºC.
Usage:
Put tablets into melting Aluminum dispersedly after skimming away the surface slag, and wait for 10 minutes , then specimen analyzing can be done after stirring for 5 minutes.
(It is better to put in tablets before putting in Silicon and Magnesium, to ensure that melting diffusion time and temperature is enough for tablets.)